Technology

Location: Home > Technology > Technology

Performance Parameter Table

2024-05-07 0

Conventional Grade

Table of Performance Parameters of Ndfel Magnets Produced by Sintering Process at Inmeng Magnette(Corperate Standard)

TypeGradeRemanenceIntrinsic Coercivity
Magnetic Coercivity
Max
Temperature Coefficient of Remanence
Coercivity Temperature Coefficient
DensityReversion- permeability
Highest Working Temperature
(Br)(Hcj)(Hcb)(BH)maxαBr≤βHcj≤ρμrecL/D=0.7
TkGskA/mkOekA/mkOekG/㎡MGOe%/℃%/℃g/cm³/
NN331.14-1.1711.4-11.7≥955≥12≥860≥10.8247-27131-340.115 0.750 7.5-7.71.03-1.0580
N351.17-1.2311.7-12.3≥955≥12≥860≥10.8263-28733-36
N381.23-1.2612.3-12.6≥955≥12≥860≥10.8287-31036-39
N401.26-1.2912.6-12.9≥955≥12≥860≥10.8302-32638-41
N421.29-1.3312.9-13.3≥955≥12≥860≥10.8318-34240-43
N451.33-1.3713.3-13.7≥955≥12≥860≥10.8342-36643-46
N481.37-1.4013.7-14.0≥955≥12≥836≥10.5358-39045-49
N501.40-1.4214.0-14.2≥955≥12≥836≥10.5374-40647-51
N521.42-1.4414.2-14.4≥955≥12≥836≥10.5390-42249-53
N541.44-1.4714.4-14.7≥955≥12≥836≥10.5406-43851-55
N561.47-1.5014.7-15.0≥955≥12≥836≥10.5422-45453-57
MN33M1.14-1.1711.4-11.7≥1114≥14≥812≥10.2247-27131-340.115 0.700 7.5-7.71.03-1.05100
N35M1.17-1.2311.7-12.3≥1114≥14≥860≥10.8263-28733-36
N38M1.23-1.2612.3-12.6≥1114≥14≥876≥11.0287-31036-39
N40M1.26-1.2912.6-12.9≥1114≥14≥907≥11.4302-32638-41
N42M1.29-1.3312.9-13.3≥1114≥14≥939≥11.8318-34240-43
N45M1.33-1.3713.3-13.7≥1114≥14≥971≥12.2342-36643-46
N48M1.37-1.4013.7-14.0≥1114≥14≥1011≥12.7358-39045-49
N50M1.40-1.4214.0-14.2≥1114≥14≥1035≥13374-40647-51
N52M1.42-1.4414.2-14.4≥1114≥14≥1003≥12.6390-42249-53
N54M1.44-1.4714.4-14.7≥1114≥14≥1003≥12.6406-43851-55
N56M1.47-1.5014.7-15.0≥1114≥14≥1003≥12.6422-45453-57
HN33H1.14-1.1711.4-11.7≥1353≥17≥844≥10.6247-27131-340.115 0.650 7.5-7.71.03-1.05120
N35H1.17-1.2311.7-12.3≥1353≥17≥876≥11.0263-28733-36
N38H1.23-1.2612.3-12.6≥1353≥17≥907≥11.4287-31036-39
N40H1.26-1.2912.6-12.9≥1353≥17≥931≥11.7302-32638-41
N42H1.29-1.3312.9-13.3≥1353≥17≥955≥12.0318-34240-43
N45H1.33-1.3713.3-13.7≥1353≥17≥995≥12.5342-36643-46
N48H1.37-1.4013.7-14.0≥1353≥17≥1019≥12.8358-39045-49
N50H1.40-1.4214.0-14.2≥1353≥17≥1035≥13374-40647-51
N52H1.42-1.4414.2-14.4≥1353≥17≥1035≥13390-42249-53
N54H1.44-1.4714.4-14.7≥1353≥17≥1035≥13406-43851-55
SHN33SH1.14-1.1711.4-11.7≥1592≥20≥836≥10.5247-27131-340.114 0.550 7.5-7.71.03-1.05150
N35SH1.17-1.2311.7-12.3≥1592≥20≥876≥11.0263-28733-36
N38SH1.23-1.2612.3-12.6≥1592≥20≥884≥11.1287-31036-39
N40SH1.26-1.2912.6-12.9≥1592≥20≥915≥11.5302-32638-41
N42SH1.29-1.3312.9-13.3≥1592≥20≥939≥11.8318-34240-43
N45SH1.33-1.3713.3-13.7≥1592≥20≥939≥11.8342-36643-46
N48SH1.37-1.4013.7-14.0≥1592≥20≥1019≥12.8358-39045-49
UHN30UH1.10-1.1411.0-11.4≥1990≥25≥756≥9.5223-24728-310.113 0.500 7.5-7.71.03-1.05180
N33UH1.14-1.1711.4-11.7≥1990≥25≥820≥10.3247-27131-34
N35UH1.17-1.2311.7-12.3≥1990≥25≥844≥10.6263-28733-36
N38UH1.23-1.2612.3-12.6≥1990≥25≥884≥11.1287-31036-39
N40UH1.26-1.2912.6-12.9≥1990≥25≥915≥11.5302-32638-41
N42UH1.29-1.3312.9-13.3≥1990≥25≥940≥11.8318-34240-43
N45UH1.33-1.3713.3-13.7≥1990≥25≥971≥12.2342-36643-46
EH33EH1.14-1.1711.4-11.7≥2388≥30≥820≥10.3247-27131-340.112 0.450 7.5-7.71.03-1.05200
35EH1.17-1.2311.7-12.3≥2388≥30≥883≥11.1263-28733-36
38EH1.23-1.2612.3-12.6≥2388≥30≥923≥11.6287-31036-39
TH28TH1.05-1.1110.5-11.1≥2786≥35≥756≥9.5207~23126~290.112 0.450 7.5-7.71.03-1.05230
30TH1.10-1.1411.0-11.4≥2786≥35≥804≥10.1223~24728~31
33TH1.14-1.1711.4-11.7≥2786≥35≥812≥10.2247-27131-34
35TH1.17-1.2311.7-12.3≥2786≥35≥844≥10.6263-28733-36

Performance Parameter Table of NdFeB in Particle Boundary Diffusion Process

Table of Performance Parameters of NdFeB Magnets Produced by Sintering Process at Jinmeng Magnetic(Corporate Standard)
Type
Grade
Remanence
Intrinsic Coercivity
Magnetic Coercivity
 Max
 Temperature Coefficient of Remanence
 Coercivity Temperature Coefficient
 Density
 Reversion- permeability
 Highest Working Temperature 
(Br)(Hcj)(Hcb)(BH)maxαBr≤βHcj≤ρμrecL/D=0.7
TkGskA/mkOekA/mkOekG/㎡MGOe%/℃%/℃g/cm³/
HN54H1.44-1.4714.4-14.7≥1353≥17≥1035≥13406-43851-550.115 0.650 7.5-7.71.03-1.05120
N56H1.47-1.5014.7-15.0≥1353≥17≥1035≥13422-45453-57
SHN45SH1.33-1.3713.3-13.7≥1592≥20≥939≥11.8342-36643-460.114 0.550 7.5-7.7150
N48SH1.37-1.3913.7-13.9≥1592≥20≥1019≥12.8358-39045-49
N50SH1.39-1.4213.9-14.2≥1592≥20≥1035≥13.0374-40647-51
N52SH1.42-1.4414.2-14.4≥1592≥20≥1059≥13.3390-42249-53
N54SH1.44-1.4714.4-14.7≥1592≥20≥1059≥13.3406-43851-55
UHN38UH1.23-1.2612.3-12.6≥1990≥25≥884≥11.1287-31036-390.113 0.500 7.5-7.7180
N40UH1.26-1.3012.6-13.0≥1990≥25≥915≥11.5302-32638-41
N42UH1.29-1.3312.9-13.3≥1990≥25≥940≥11.8318-34240-43
N45UH1.33-1.3713.3-13.7≥1990≥25≥971≥12.2342-36643-46
N48UH1.37-1.4013.7-14.0≥1990≥25≥1011≥12.7358~39045-49
N50UH1.4-1.4214.0-14.2≥1990≥25≥1035≥13374~40647-51
N52UH1.42-1.4414.2-14.4≥1990≥25≥1035≥13390-42249-53
N54UH1.44-1.4714.4-14.7≥1990≥25≥1035≥13406-43851-55
EH38EH1.23-1.2612.3-12.6≥2388≥30≥923≥11.6287-31036-390.112 0.450 7.5-7.7200
40EH1.26-1.3012.6-13.0≥2388≥30≥947≥11.9295~32637~41
42EH1.29-1.3312.9-13.3≥2388≥30≥971≥12.2310~34239~43
45EH1.32-1.3713.2-13.7≥2388≥30≥987≥12.4334-36642-46
48EH1.37-1.4013.7-14.0≥2388≥30≥1011≥12.7358-39045-49
TH33TH1.14-1.1711.4-11.7≥2786≥35≥812≥10.2247-27131-340.112 0.450 230
35TH1.17-1.2311.7-12.3≥2786≥35≥844≥10.6263-28733-36
38TH1.23-1.2612.3-12.6≥2786≥35≥923≥11.6287-31036-39
40TH1.26-1.3012.6-13.0≥2786≥35≥939≥11.8295~32637~41
42TH1.29-1.3312.9-13.3≥2786≥35≥939≥11.8310~34239~43

Illustrate

1.The main magnetic performance test methods for N,M,H,SH,and UH materials shall be carried out in accordance with the provisions of GB/T3217,while the main magnetic performance test methods for EH and TH materials shall be carried out in accordance with the provisions of GB/T29628.

2.The test method for the temperature coefficient of residual magnetism and intrinsic coercive force of materials shall be carried out in accordance with the provisions of GB/T24270.

3.The temperature coefficient in the table corresponds to a temperature range of 20-80 degrees Celsius in the N range;M gear 20-100 degrees Celsius;H-range 20-120 degrees Celsius;SH range 20-150 degrees Celsius;UH range 20-180 degrees Celsius;EH range 20-200 degrees Celsius;TH gear 20-230 degrees Celsius.

Performance Table of Bonded NdFeB

Magnetic Properties of Bonded NdFeB Permanent Magnets at Room Temperature (20℃)
Material Grade
BrHcjHcb(BH)max
BNM-4350-570mT
3500-5700Gs
480-720kA/m
6000-9000Oe
240-320kA/m
3000-4000Oe
28-44kJ/m
3.5-5.5MGOe
BNM-6580-630mT
5800-6300Gs
640-800kA/m
8000-10000Oe
320-376kA/m
4000-47000e
44-56kJ/m
5.5-7.0MGOe
BNM-8620-670mT
6200-6700Gs
640-800kA/m
8000-10000Oe
360-432kA/m
4500-5400Oe
56-70kJ/m
7.0-8.7MGOe
BNM-9640-690mT
6400-6900Gs
640-800kA/m
8000-100000e
410-464kA/m
5100-5800Oe
68-76kJ/m
8.5-9.5MGOe
BNM-10650-700mT
6500-7000Gs
640-800kA/m
8500-10000Oe
416-480kA/m
5200-6000Oe
72-80kJ/m
9.0-10.0MGOe
BNM-11680-720mT
6800-7200Gs
720-840kA/m
9000-10500Oe
422-496kA/m
5200-62000e
80-88kJ/m
10.0-11.0MGOe
BNM-11L690-740mT
6900-7400Gs
520-640kA/m
6500-80000e
400-464kA/m
5000-58000e
80-88kJ/m
10.0-11.0MGOe
BNM-12L720-760mT
7200-7600Gs
520-640kA/m
6500-8000Oe
424-480kA/m
5300-60000e
84-92kJ/m
10.5-11.5MGOe
BNM-8SR620-670mT
6200-6700Gs
880-1120kA/m
11000-14000Oe
400-464kA/m
5000-58000e
64-78kJ/m
8.0-9.5MGOe
BNM-12720-770mT
7200-7700Gs
720-840kA/m
9000-10500Oe
456-512kA/m
5700-64000e
88-96kJ/m
11.0-12.0MGOe
BSM-7560-630mT
5600-6300Gs
720-840kA/m
9000-10500Oe
359-420kA/m
4400-52000e
52-60kJ/m
6.5-7.5MGOe