By using technologies such as PVD,CVD,or printing,DY,Tb,Pr,and other alloys are difiused from the surface of the magnet to the interior of the magnet by heat at around 900 ℃,forming a high coercivity shell layer on the grain surface to significantly increase the coercivity of the magnet without reducing residual magnetism